| TECHNICAL
DATA |
| Purity/sulphur
content max. ASTM C-816 |
98% / 700ppm |
| Bulk density
ASTM C-559 |
1.0 to 1.1
g/cc |
| Ash content
ASTM C-561 |
Less than
0.5% |
| Leachable
chloride/fluorides |
50ppm max.
ASTM D-512 |
| Temperature
range |
-200°C to
3000°C Non-oxidizing |
| |
-200°C to
+500°C Oxidizing |
| |
-200°C to
+650°C Steam |
| Tensile
strength/stress relaxation |
998Psi / DIN
52913 - 48N/mm2 |
| Shore
hardness (D) / Creep relaxation |
30 / At
100°C ASTM F-38 < 5% |
| Sealability,
ml/h Fuel A ASTM F-37B |
< 0.2 to
0.5 |
| Electrical
resistance |
900 x 10-6
ohm cm parallel to surface |
| |
250,000 x 10-6
ohm cm perpendicular to surface |
| Thermal
conductivity |
120 Kcal/m.
Hr°C parallel to surface |
| |
4 Kcal/m.
Hr°C perpendicular to surface |
| Coefficient
of Thermal Expansion |
5 x 10-6
/ °C parallel to surface |
| |
2 x 10-6
/ °C perpendicular to surface |
| Compressive
strength |
more than
800kg/cm2 |
| Ignition
loss / operating pressure |
less than 1%
/ 140 bar (2058p.s.i) |
| Resilient
rate / density |
more than
30% / 0.7 to 1.1 g/cu.cm |
| Compressibility
Strength ASTM F36A-66 |
40 to 45% |
| Recovery
ASTM F36A-66 |
20 to 40% |
| ASTM
"m" factor |
2 |
| ASTM
"y" stress |
1500 Psi |
| Sliding-frictional
coefficient |
0.149 |
| Permeability
coefficient for air |
less than 2
x 10-5 cm2/sec perpendicular to surface |
| pH Range |
less than 2
x 10-5 cm2/sec perpendicular to surface |
| Oxidation
rate exposed edge at 500°C |
0.03 to 0.4
g/cm2/h |